适用范围:
电子、微电子、通讯、计算机、精密仪器、纺织、印刷、粉体、化学、有机溶剂、瓦斯等一切需要抗静电的工厂的墙面、地坪及储油罐区域。
Application Scope:
The wall surfaces, floors and oil reservation tanks areas that shall be anti-static for such industries as electronics, micro-electronics, communication, computer, complicated apparatus, textile, Imprinting, powder, organic solvent, gas and so on.
性能特点:
·抗静电效果优良持久
·防潮耐磨,不受时间、温度、湿度等影响
·表面光洁平整
Performances and Features:
·Excellent and lasting anti-static ability.
·Damp-proof, endurable, not affected by time, temperature, humidity and etc.
·Smooth and light surface.
施工工艺:
·基面处理
·滚防静电底漆
·铺设导电铜箔并做接地
·刮防静电砂浆中涂
·镘涂防静电腻子
·滚涂或喷涂防静电薄涂面漆
Construction Techniques:
·Ground or wall surface treatment.
·Coating conductive primer.
·Lay grounding copper line.
·Fill the seams the copper line leaves with conductive putty.
·Coat intermediate paint.
·Spray anti-static finished paint.
技术指标Technical Index :
测试项目 Test Items | 指标 Index |
表干h Surface Dry (h) | ≤4 |
实干h Actual Dry(h) | ≤24 |
附着力(级) Adhesion (Class) | ≤2 |
铅笔硬度(H) Pencil Rigidity(H) | ≥2 |
耐冲击性(Kg) Impact Resistance(Kg) | 50通过 50 Passed |
展开表格
优点;
1.恒久不变的防静电功能
2.镜面般光滑的表面
3.抗压耐磨,寿命持久
4.可承受中型荷载
缺点;
1.色彩没有防静电自流平地坪饱满
2.使用年限都没有耐磨地坪时间长;
养护:
1.防静电坪地施工完毕后需养护2-3天后方可投入使用,在养护期间,应避免水或其它溶液侵润表面
2.凡进入车间员工必须要换成胶底鞋
3.凡是硬件:如铁椅、铁桌,须将其脚用软质塑料、像胶包裹或用纸皮垫起来以免在使用过程中划伤地面
4.可根据地面要求做打蜡处理
混凝土裂缝修补方法:
1.表面修补:
表面修补法是一种简单,常见的修补方法,它主要适用于稳定和对结构承载能力,没有影响的表面裂缝以及深进裂缝处理。通常的处理措施是在裂缝的表面涂抹水泥浆,环氧胶泥或在混凝土表面涂刷油漆。在防护的同时为了防止混凝土受各种作用的影响继续开裂,通常可以采用在裂缝的表面黏贴玻璃纤维布等措施。
裂缝处理
1.如裂缝是由于结构本身的问题而产生的结构受力裂缝,要对结构进行加固补强修复,如裂缝为非结构受力裂缝。